降色温玻璃特性
牌 号 | 厚度 (mm) | A[2856k] | D65 | 化学稳定性 | ND | α×10-7 (/℃) | Tg (℃) | Ts (℃) | S | |||||
x | y | Y | x | y | Y | DA | DW | |||||||
SJB20 | 2 | 0.469 | 0.413 | 87.8 | 0.339 | 0.349 | 83.6 | 2 | 3 | 1.525 | 87 | 571 | 642 | 2.63 |
SJB80 | 2 | 0.494 | 0.415 | 75.3 | 0.372 | 0.368 | 69.2 | 2 | 3 | 1.525 | 87 | 571 | 642 | 2.63 |
SJB100 | 2 | 0.510 | 0.410 | 67.8 | 0.395 | 0.381 | 61.0 | 2 | 3 | 1.525 | 103 | 513 | 591 | 2.70 |
降色温玻璃技术要求
牌 号 | 厚度 (mm) | V(Mired) | |
标准 | 公差 | ||
SJB20 | 2 | 20 | 20±2 |
SJB80 | 2 | 80 | 80±8 |
SJB100 | 2 | 100 | 100±10 |
降色温玻璃气泡、条纹、应力类级别
牌 号 | 气 泡 | 条 纹 | 应 力 |
SJB20 | C | 3C | 3 |
SJB80 | C | 3C | 3 |
SJB100 | C | 3C | 3 |
降色温玻璃特性
牌 号 | 厚度 (mm) | A[2856k] | D65 | 化学稳定性 | ND | α×10-7 (/℃) | Tg (℃) | Ts (℃) | S | |||||
x | y | Y | x | y | Y | DA | DW | |||||||
SJB130 | 2 | 0.548 | 0.409 | 52.1 | 0.455 | 0.405 | 44.2 | 2 | 3 | 1.525 | 103 | 513 | 591 | 2.70 |
SJB140 | 2 | 2 | 3 | 1.525 | 103 | 513 | 591 | 2.70 |
降色温玻璃技术要求
牌 号 | 厚度 (mm) | V(Mired) | |
标准 | 公差 | ||
SJB130 | 2 | 130 | 130±13 |
SJB140 | 2 | 140 | 140±14 |
降色温玻璃气泡、条纹、应力类级别
牌 号 | 气 泡 | 条 纹 | 应 力 |
SJB130 | C | 3C | 3 |
SJB140 | C | 3C | 3 |
拥有30多年的丰富经验和技术研发能力,致力于成为引领并推动国际光学的行业发展的领导者;
与央视合作,一直秉承“不断满足客户需求,提升企业社会价值,追求完美设计,完善自我”的经营理念。
严格按照IS09001质量规范组织开展生产、销售、服务。
拥有50多台套光学玻璃精密数控加工;
原料、切割、磨边、打孔、研磨、抛光、清洗、钢化热处理等工序全程严密管控。
以“诚信为基础,以互惠互利”为宗旨;
根据客户不同的需求来图定制,满足客户需求;
精心包装注重每个发货细节,海陆空为客户提供最具性价比的物流配送。
我要咨询: